Volumizing Mascara With SPC/BLACK NF-I2 KMA-035

Kobo Products

This long-wear mascara contains Kobo's Carbon Black dispersion, WSJ10CB, for intense, deep, black color. Kobo's pigmentary dispersion, W60BBNFAP, is used in combination with WSJ10CB to provide the deep black shade and add film-forming properties. Kobo's resin composite, Koboguard® 5400 SQ, gives quick build up with a water-resistant film, and aids in long wear. SPC/BLACK NF-I2 hollow Microsphere complex with ITT adds building effect to the lashes.

Phase
Product
INCI Name
Supplier
Volume
A

Beeswax White SP 422

Beeswax

Strahl & Pitsch, Inc.

8.00

Ozokerite Wax White SP 1020

Ozokerite

Strahl & Pitsch, Inc.

5.00

Carnauba Wax SP 63

Copernicia Cerifera (Carnauba) Wax

Strahl & Pitsch, Inc.

3.00

Dermofat 4919

Stearic Acid

Alzo International Inc.

3.00

Microcrystalline Wax SP-89

Microcrystalline Wax

Strahl & Pitsch, Inc.

3.00

KOBOGUARD® 5400 SQ

Hydrogenated Polycyclopentadiene (And) Squalane

Kobo Products

2.00

Liposorb® SQO

Sorbitan Sesqioleate

Lipo Chemicals

1.00

Propyl Paraben NF

Propylparaben

0.10

B

Deionized Water

Water

33.15

W60BBNFAP

Iron Oxides (C.I. 77499) (And) Water (And) Ammonium Polyacrylate

Kobo Products

15.00

TEAlan 99%

TriethanolAmine

RITA Corp.

1.00

Natrosol® 250 HHR

Hydroxyethylcellulose

Hercules-Aqualon

0.30

Methyl Paraben NF

Methylparaben

0.20

C

Deionized Water

Water

6.00

Jeecide CAP-5

Phenoxyethanol (And) Caprylyl Glycol (And) Potassium Sorbate (And) Water (And) Hexylene Glycol

Jeen International

0.60

Germall® 115

Imidazolidinyl Urea

ISP

0.15

D

WSJ10CB

Black 2 (And) PEG-40 Hydrogenated Castor Oil (And) Water (And) Acrylates/Ethylhexyl Acrylate Copolymer (And) Aminomethyl Propanol (And) Sodium Dehydroacetate (And) Sodium Acrylate/Sodium Acryloyldimethyl Taurate Copolymer (And) Laureth-21

Kobo Products

15.00

SPC/BLACK NF-I2

Iron Oxides (C.I. 77499) (And) Ethylene/Methacrylate Copolymer (And) Isopropyl Titanium Triisostearate

Kobo Products

3.50

Preparation:

  1. Heat Part 1 to 80°C in auxiliary tank.
  2. Heat Part 2 to 80°C in main tank.
  3. Add Part 1 to Part 2 in main tank with propeller and sweep agitation at 80°C.
  4. Cool to 50°C.
  5. Add Part 3 ingredients at 50°C.
  6. Add Part 4 at 45°C.
  7. Cool to 25-27°C.
Disclaimer

While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.

Latest Issues

NYSCC Suppliers' Day 2026

Javits Center, New York
19 - 20 May

in-cosmetics Korea 2026

COEX, Seoul
1 - 3 July 2026