Jarchemtm Double Black Diamond Firming Clay Mask

Aurorium

Formula No. AK01046

Phase
Product
INCI Name
Supplier
Volume
A

Water

Water

59.86

Magnesium Aluminum Silicate

Magnesium Aluminum Silicate

Vanderbilt

4.50

B

Zemea™

Propanediol

Dupont Tate & Lyle Bioproducts

2.50

Glycerin

Glycerin

2.50

Xanthan Gum

Xanthan Gum

0.24

C

Jarxotic™ BLACK DIAMOND CLAY

Illite (and) Quartz (and) Kaolin

Jarchem

29.4

D

Euxyl™ K940

Phenoxyethanol (and) Benzyl Alcohol (and) Ethylhexylglycerin

Schülke

1.0

Preparation:

Procedure: 1. Add water to main vessel and heat to 65-70°C. Sprinkle in Magnesium Aluminum Silicate and mix for 15 minutes. 2. In a separate vessel, mix Phase B. 3. Remove Phase A from heat, and add Phase B to Phase A while mixing. 4. Add Phase C ingredients one at a time while mixing. 5. Add Phase D and mix.

Disclaimer

While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.