CREAM TO POWDER FOUNDATION

Cargill Beauty

This unique, non-volatile, low silicone foundation applies with a creamy texture and finishes with a powder-dry feel. Floramac 10 provides the dry emollient feel and, unlike cyclopentasiloxane materials, is naturally derived and will not evaporate after application.

Phase
Product
INCI Name
Supplier
Volume
A

Floramac 10

Ethyl Macadamiate

Floratech

29.33

SF 1550

Phenyl Trimethicone

Momentive Performance Materials

1.00

Permethyl® 102A

Isoeicosane

Presperse Corporation

q.s

Dow Corning® 9506 Powder

Dimethicone/Vinyl Dimethicone Crosspolymer

Dow Corning Corporation

1.50

B

Performalene® 400 Polyethylene

Polyethylene

New Phase Technologies / Baker Hughes

3.65

Candelilla Wax SP 75

Euphorbia Cerifera (Candelilla) Wax

Strahl & Pitsch Inc.

2.36

Syncrowax HR-C

Tribehenin

Croda, Inc.

0.50

Microcrystalline Wax SP 18

Microcrystalline Wax

Strahl & Pitsch Inc.

1.60

C

Titanium Dioxide (Oil Dispersed)

Titanium Dioxide

Emerald Performance Materials

14.50

Unipure LC® Yellow 182

Iron Oxides

Sensient Cosmetic Technologies

1.50

Pur Oxy Black BC (34PC3190E)

Iron Oxides

Emerald Performance Materials

0.15

Unipure LC® Red 381

Iron Oxides

Sensient Cosmetic Technologies

0.45

RonaFlair® White

Sodium Potassium Aluminum Silicate (and) Silica (and) Titanium Dioxide

EMD Chemicals

11.00

Tres BN® PHP1109

Boron Nitride

Saint-Gobain Advanced Ceramics

0.50

Ganzpearl® GM-0600

Polymethyl Methacrylate

Presperse Corporation

5.50

Spheron P-1500

Silica

Presperse Corporation

3.50

Natrasorb® HFB

Aluminum Starch Octenylsuccinate (and) Acrylates Copolymer (and) Magnesium Carbonate

AkzoNobel Chemicals

5.50

D

Eusolex® 2292

Ethylhexyl Methoxycinnamate (and) BHT

EMD Chemicals

6.20

Oxybenzone, USP

Benzophenone-3

Essential Ingredients

2.06

Preservative1



q.s

Covi-Ox® T 70 C

Tocopherol

BASF Corporation

0.10

RTD Alpha-Bisabolol Natural

Bisabolol

The HallStar Company

0.20

Preparation:

Mixing Procedure

  1. Mix Phase A at 85-90°C with propeller agitation.
  2. Mix all components of Phase B at 95°C and stir until homogeneous. Add Phase B to Phase A and keep the temperature of the mixture at 90°C.
  3. With the aid of a homomixer, add each ingredient of Phase C to Phase AB. Continue to homomix this combination at 90°C to ensure uniform pigment dispersion.
  4. Mix all components of Phase D at 70°C. Cool Phase ABC down to 70°C and add Phase D with homomixing agitation.
  5. Pour final mixture, while hot in liquid form, into containers and cool to room temperature.

Notes:

Typical Properties:
Relative Strength: 0.15 - 0.3 kg
Penetration: 175 - 250 dmm

Disclaimer

While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.