Broad Spectrum SPF ~49, PFA (PPD) ~17, Sunscreen Cream Formula CAB6-159, Batch JZ2-29
Hallstar
HallBrite ® OS
Ethylhexyl Salicylate [Octisalate]
5.000
HallBrite ® HS USP
Homosalate [Homosalate]
7.500
Neo Heliopan ® 303
Octocrylene [Octocrylene]
2.750
Spectrasolv ® DMDA
Dimethyl Capramide
1.000
Polycrylene ®
Polyester-8
3.000
Neo Heliopan ® BB
Benzophenone-3 [Oxybenzone]
4.000
Neo Heliopan ® 357
Butyl Methoxydibenzoylmethane [Avobenzone
3.000
HallStar ® TA-1618 Cetearyl Alcohol
Cetearyl Alcohol
0.350
HallStar ® GMS SE/AS
Glyceryl Stearate (and) PEG-100 Stearate
2.500
Performa V ® 1608 LM
C30-38 Olefin/Isopropyl Maleate/MA Copolymer
0.800
Emulsiphos ™
Potassium Cetyl Phosphate, Hydrogenated Palm Glycerides
1.500
Deionized
Water
47.100
Versene ™ NA
Disodium EDTA
0.100
Trolamine 99, N.F.
Triethanolamine
0.600
1,3-Butylene Glycol
Butylene Glycol
4.000
CoSept ™ PEP
Phenoxyethanol, Methylparaben, Ethylparaben, Butylparaben, Propylparaben, Isobutylparaben
0.600
Deionized
Water
4.000
Carbopol ® Ultrez ™ 10
Carbomer
0.200
Deionized
Water
4.143
Sodium Hydroxide
Sodium Hydroxide (99%)
0.212
Neo Heliopan ® Hydro
Phenylbenzimidazole Sulfonic Acid
1.500
Benzyl Alcohol, ACS, 99+%
Benzyl Alcohol
0.500
Simulgel ™ 600
Acrylamide/Sodium Acryloyldimethyltaurate Copolymer, Isohexadecane, Polysorbate 80
1.750
Dry-Flo ® PC
Aluminum Starch Octenylsuccinate
2.500
Preparation:
In secondary vessel combine 1-5, start mixing, add 6 & 7, heat to 95°C, and then add 8-11, in order, to this oil phase. To the main vessel add 12, start mixing, add 13 and heat to 90°C. Meanwhile, in a separate vessel combine 14, 15 and 16 and mix to homogeneity. In another vessel, disperse 18 in 17 and maintain in suspension. In yet another vessel combine, in order, with continued mixing until a homogeneous solution, 19-21. When oil and water phases are uniform and at the defined temperatures, add 22 to the oil phase, mix well, and then add the oil phase to the water phase with strong mixing without aeration. Remove from heat. After ten minutes, start homogenizing and add the dispersion of 18 in 17. After homogenizing for ten minutes, stop homogenizing, start sweep mixing, and continue cooling batch. Add solution of 14-16, then solution of 19-21, then 23, and finally add 24. Add water if necessary to correct for evaporative losses. Stop cooling and mixing when homogeneous and at desired filling temperature. Perform quality assurance checks.
Notes:
PRODUCT CHARACTERISTICS (23°C) Appearance: opaque white cream Viscosity (Brookfield, Model RV, T-Bar E, 5, 20 & 100 rpm; cP): 30000, 10000 & 3140 pH: 6.8
Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
Our company was established in 1958 as SEIWA KASEI Industry CO., LTD., an organization for the development of industrial decomposition technology of waxes and high melting point esters such as Beeswax, Privet wax, and Carnauba wax, and for the production of various types of emulsifying waxes. In 1966, we launched our products, hydrolyzed...